The University of Nevada at Reno proposes to propose to develop mitigation of the possible initiation of pitting/stress corrosion cracking (SCC) in…
Office of NEPA Policy and Compliance
August 10, 2020The University of Nevada at Reno proposes to propose to develop mitigation of the possible initiation of pitting/stress corrosion cracking (SCC) in dry storage canisters austenitic stainless-steel welds by applying laser shock peening, shot peening and ultrasonic impact peening as well as indirect laser shock surface patterning methods (LSSP).